General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | ASTM D 570 | (23°C/24hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 30 % Show Supplier Material materials with Elongación of 30 % | ASTM D 638 | brk, Type I, 50 mm/min |
Módulo de flexión | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Resistencia a la flexión | 23.0 °C | 75 MPa Show Supplier Material materials with Resistencia a la flexión of 75 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Resistencia a la tracción | 23.0 °C | 49 MPa Show Supplier Material materials with Resistencia a la tracción of 49 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 234 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 234 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 7.38E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 7.38E-5 1/K | ASTM E 831 | 0°C to 100°C |
Heat deflection temperature, 0.45 MPa | 121 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 121 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 112 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 112 °C | ASTM D 648 | 6.4 mm, unannealed | |
Temperatura de flexión bajo carga | 112 - 121 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 112 - 121 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Contracción | 23.0 °C | 0.5 % Show Supplier Material materials with Contracción of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Motorcycle, Refrigerator, Photovoltaic Components, Plumbing, Wearables, Wiring Devices, Auto Electrical, Audio, Auto Aftermarket, Data Management, Data Transfer, Document Handling, Drain Pan, Gas/Electric Oven, Heavy Vehicles, Hygiene/Personal Care, Food Transportation, Enclosures, Enclosure/Housing/Cover, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Nozzle Temperature: 275 to 305.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |