Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 6 % Show Supplier Material materials with Elongación of 6 % | ISO 527 | break, 50 mm/min |
Módulo de flexión | 23.0 °C | 3 GPa Show Supplier Material materials with Módulo de flexión of 3 GPa | ISO 178 | 2 mm/min |
Módulo elástico | 23.0 °C | 3.1 GPa Show Supplier Material materials with Módulo elástico of 3.1 GPa | ISO 527 | 1 mm/min |
Resistencia a la flexión | 23.0 °C | 130 MPa Show Supplier Material materials with Resistencia a la flexión of 130 MPa | ISO 178 | yield, 2 mm/min |
Resistencia a la tracción | 23.0 °C | 86 MPa Show Supplier Material materials with Resistencia a la tracción of 86 MPa | ISO 527 | yield, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 3 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 163 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 163 °C | ISO 75/Be | Edgew 120*10*4 sp=100mm |
Heat deflection temperature, 1.80 MPa | 147 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 147 °C | ISO 75/Ae | Edgew 120*10*4 sp=100mm |
Temperatura de flexión bajo carga | 147 - 163 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 147 - 163 °C | |
Temperatura de reblandecimiento Vicat | 174 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 174 °C | ISO 306 | Rate A/50 |
Technological properties
Property | ||
---|---|---|
Application areas | Bottles, Audio, Additive Semiconductor Materials, Food Container, Electronic Components | |
Availability | Europe,Asia,Americas | |
Processing methods | Melt Temperature: 280 to 300.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |