General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad relativa | 23.0 °C | 1.03 [-] Show Supplier Material materials with Densidad relativa of 1.03 [-] | ASTM D 792 | |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Shore A | 23.0 °C | 89 [-] Show Supplier Material materials with Dureza Shore A of 89 [-] | ASTM D 2240 | 30S reading |
Elongación | 23.0 °C | 210 % Show Supplier Material materials with Elongación of 210 % | ISO 527 | break, 50 mm/min |
Módulo de flexión | 23.0 °C | 0.1 GPa Show Supplier Material materials with Módulo de flexión of 0.1 GPa | ISO 178 | 12.5 mm/min |
Resistencia a la tracción | 23.0 °C | 18 MPa Show Supplier Material materials with Resistencia a la tracción of 18 MPa | ISO 527 | break, 50 mm/min |
Aplicaciones térmicas
Property | Value | Comment | |
---|---|---|---|
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | IEC 60695-2-13 | 3.0 mm | |
Inflamabilidad | Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 3mm IEC 60695-2-12 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 4.70E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 4.70E+15 Ω·cm | IEC 60093 |
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | IEC 60112 | |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 17 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 17 g/10min | ASTM D 1238 | 250°C/10.0 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Power Manangement, Heavy Vehicles, Wire & cable | |
Availability | Asia | |
Processing methods | Cooling Water Air Gap: 100 to 200.0mm | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |