General
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 7.5 % Show Supplier Material materials with Elongación of 7.5 % | ASTM D 638 | yld, Type I, 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 578 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 578 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2140 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 2140 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 77 J Show Supplier Material materials with Instrumented Impact, Total Energy of 77 J | ASTM D 3763 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 73 J Show Supplier Material materials with Instrumented Impact, at Peak of 73 J | ASTM D 3763 | 23°C |
Módulo de flexión | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo de flexión of 2.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Módulo elástico | 23.0 °C | 2.2 GPa Show Supplier Material materials with Módulo elástico of 2.2 GPa | ASTM D 638 | 50 mm/min |
Resistencia a la flexión | 23.0 °C | 105 MPa Show Supplier Material materials with Resistencia a la flexión of 105 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Resistencia a la tracción | 23.0 °C | 68 MPa Show Supplier Material materials with Resistencia a la tracción of 68 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 578 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 578 kJ/m² | ASTM D 256 | notched, 23°C |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Ball Pressure Test | PASS | IEC 60695-10-2 | 125°C +/- 2°C |
Heat deflection temperature, 0.45 MPa | 160 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 160 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 147 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 147 °C | ASTM D 648 | 3.2mm, unannealed |
Temperatura de flexión bajo carga | 147 - 160 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 147 - 160 °C | |
Temperatura de reblandecimiento Vicat | 164 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 164 °C | ASTM D 1525 | Rate B/50 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Velocidad de flujo de la masa derretida | 15 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 15 g/10min | ASTM D 1238 | 330°C/2.16 kgf |
Technological properties
Property | ||
---|---|---|
Application areas | Enclosures | |
Availability | Europe,Americas | |
Processing methods | Melt Temperature: 350 to 370.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |