General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Densidad of 1.33 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Impact strength, Izod notched, ASTM | 23.0 °C | 130 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 130 J/m | ASTM D 256 | notched, 23°C |
Módulo de flexión | 23.0 °C | 8.9 GPa Show Supplier Material materials with Módulo de flexión of 8.9 GPa | ASTM D 790 |
Resistencia a la flexión | 23.0 °C | 268 MPa Show Supplier Material materials with Resistencia a la flexión of 268 MPa | ASTM D 790 |
Resistencia a la tracción | 23.0 °C | 176 MPa Show Supplier Material materials with Resistencia a la tracción of 176 MPa | ASTM D 638 | break |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 130 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 130 kJ/m² | ASTM D 256 | notched, 23°C |
Technological properties
Property | ||
---|---|---|
Availability | Asia,Americas | |
Processing methods | Front - Zone 3 Temperature: 270 to 280.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |