General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 23.0 °C | 1.16 % Show Supplier Material materials with Absorción de agua of 1.16 % | ASTM D 570 | (23°C/Saturated) |
Densidad | 23.0 °C | 1.29 g/cm³ Show Supplier Material materials with Densidad of 1.29 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.23 % Show Supplier Material materials with Moisture absorption of 0.23 % | ASTM D 570 | (50% RH, Equilibrium) |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Material | |
Availability | Europe,Asia,MEA,Americas,Global | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |