ULTEM™ Resin AR9300 - Americas

Want to keep this datasheet? Save it now in your required format

Description

30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming.

Los datos sobre este material han sido proporcionados por Sabic.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

Propiedades

Mecánica

PropertyTemperatureValueComment

Elongación

23.0 °C

3 %

Show Supplier Material materials with Elongación of 3 %

ASTM D 638 | brk, Type I, 5 mm/min

Módulo de flexión

23.0 °C

9.7 GPa

Show Supplier Material materials with Módulo de flexión of 9.7 GPa

ASTM D 790 | 2.6 mm/min, 100 mm span

Módulo elástico

23.0 °C

9 GPa

Show Supplier Material materials with Módulo elástico of 9 GPa

ASTM D 638 | 5 mm/min

Resistencia a la flexión

23.0 °C

241 MPa

Show Supplier Material materials with Resistencia a la flexión of 241 MPa

ASTM D 790 | yld, 2.6 mm/min, 100 mm span

Resistencia a la tracción

23.0 °C

155 MPa

Show Supplier Material materials with Resistencia a la tracción of 155 MPa

ASTM D 638 | brk, Type I, 5 mm/min

Aplicaciones térmicas

PropertyValueComment

Heat deflection temperature, 1.80 MPa

212 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 212 °C

ASTM D 648 | 6.4 mm, unannealed

Temperatura de flexión bajo carga

212 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 212 °C

Inflamabilidad

Vertical Burn b (12s) passes at: 0sec FAR 25.853 <br> NBS Smoke Density, Flaming, Ds 1.5 min: 0- ASTM E 662 <br> OSU peak heat release rate (5 minute test): 40kW/m² FAR 25.853 <br> Vertical Burn a (60s) passes at: 0sec FAR 25.853 <br> NBS Smoke Density, Flaming, Ds 4 min: 5- ASTM E 662 <br> NBS Smoke Density, Flaming, Dmax: 5- ASTM E 662 <br> FAA Flammability, FAR 25.853 A/B: NATURAL- FAR 25.853

Rheological Properties

PropertyTemperatureValueComment

Contracción

23.0 °C

0.2 %

Show Supplier Material materials with Contracción of 0.2 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Enclosure/Housing/Cover, Air Cabin Interiors, Aircraft Seating, Aerospace

Availability

Europe,Asia,Americas

Processing methods

Maximum Moisture Content: 0.02%
Shot to Cylinder Size: 40 to 60.0%
Vent Depth: 0.025 to 0.076mm
Mold Temperature: 135 to 165.0°C
Screw Speed: 40 to 70.0rpm
Back Pressure: 0.3 to 0.7MPa
Nozzle Temperature: 360 to 380.0°C
Rear - Zone 1 Temperature: 345 to 365.0°C
Drying Time: 4 to 6.0hrs
Drying Temperature: 150°C
Drying Time (Cumulative): 24hrs
Front - Zone 3 Temperature: 365 to 390.0°C
Melt Temperature: 365 to 390.0°C
Middle - Zone 2 Temperature: 355 to 375.0°C

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.