General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 0.05 g/cm³ Show Supplier Material materials with Densidad of 0.05 g/cm³ | ASTM D 1622 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo de cizallamiento | 23.0 °C | 0 GPa Show Supplier Material materials with Módulo de cizallamiento of 0 GPa | ASTM C 273 |
Módulo de compresión | 23.0 °C | 22 MPa Show Supplier Material materials with Módulo de compresión of 22 MPa | |
Módulo de compresión transversal | 23.0 °C | 22 MPa Show Supplier Material materials with Módulo de compresión transversal of 22 MPa | ASTM D 1621 |
Módulo elástico | 23.0 °C | 0 GPa Show Supplier Material materials with Módulo elástico of 0 GPa | ASTM D 638 |
Resistencia a la compresión transversal | 23.0 °C | 0.5 MPa Show Supplier Material materials with Resistencia a la compresión transversal of 0.5 MPa | ASTM D 1621 |
Resistencia al cizallamiento | 23.0 °C | 0.6 MPa Show Supplier Material materials with Resistencia al cizallamiento of 0.6 MPa | ASTM C 273 |
Aplicaciones térmicas
Property | Value |
---|---|
Inflamabilidad | OSU peak heat release rate (5 minute test): <55kW/m² FAR 25.853 <br> Smoke Density: <10Ds FAR 25.853 <br> Smoke Toxicity: PASSES- OEM BSS <br> Smoke Toxicity: PASSES- OEM ABD <br> Insulation Radiant Panel: PASSES- FAR 25.856 <br> Vertical Burn at 60 Seconds: PASSES- FAR 25.853 <br> Flame Spread at 1" Thick: <25- ASTM E 84 <br> Smoke Developed at 1" Thick: <50- ASTM E 84 |
Technological properties
Property | ||
---|---|---|
Application areas | Panels, Air Cabin Interiors, Composite | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |