General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.4 g/cm³ Show Supplier Material materials with Densidad of 8.4 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Sheet Thickness: 0.3 - 8 mm, Foil Thickness: 0.005-0.45 mm |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 55 [-] Show Supplier Material materials with Dureza Brinell of 55 [-] |
Elongación A5 | 23.0 °C | 48 % Show Supplier Material materials with Elongación A5 of 48 % |
Límite elástico Rp 0,2 | 23.0 °C | 180 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 180 MPa |
Módulo elástico | 23.0 °C | 110 GPa Show Supplier Material materials with Módulo elástico of 110 GPa |
Resistencia a la tracción | 23.0 °C | 300 MPa Show Supplier Material materials with Resistencia a la tracción of 300 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.02E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.02E-5 1/K |
Conductividad térmica | 23.0 °C | 121 W/(m·K) Show Supplier Material materials with Conductividad térmica of 121 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.55E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.55E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.05 % Show Supplier Material materials with Aluminio of 0.05 % |
Cobre | 62 - 64 % Show Supplier Material materials with Cobre of 62 - 64 % |
Estaño | 0.1 % Show Supplier Material materials with Estaño of 0.1 % |
Hierro | 0.1 % Show Supplier Material materials with Hierro of 0.1 % |
Níquel | 0.3 % Show Supplier Material materials with Níquel of 0.3 % |
Plomo | 0.1 % Show Supplier Material materials with Plomo of 0.1 % |