General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.5 g/cm³ Show Supplier Material materials with Densidad of 7.5 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 180 [-] Show Supplier Material materials with Dureza Brinell of 180 [-] |
Elongación A5 | 23.0 °C | 15 % Show Supplier Material materials with Elongación A5 of 15 % |
Límite elástico Rp 0,2 | 23.0 °C | 270 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 270 MPa |
Módulo elástico | 23.0 °C | 127 GPa Show Supplier Material materials with Módulo elástico of 127 GPa |
Resistencia a la tracción | 23.0 °C | 640 MPa Show Supplier Material materials with Resistencia a la tracción of 640 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K |
Conductividad térmica | 23.0 °C | 39 W/(m·K) Show Supplier Material materials with Conductividad térmica of 39 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 6.00E+6 S/m Show Supplier Material materials with Conductividad eléctrica of 6.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 9 - 11 % Show Supplier Material materials with Aluminio of 9 - 11 % |
Cobre | 76.8 - 85 % Show Supplier Material materials with Cobre of 76.8 - 85 % |
Estaño | 0 - 0.2 % Show Supplier Material materials with Estaño of 0 - 0.2 % |
Hierro | 2 - 4 % Show Supplier Material materials with Hierro of 2 - 4 % |
Manganeso | 0 - 1.5 % Show Supplier Material materials with Manganeso of 0 - 1.5 % |
Níquel | 4 - 5.5 % Show Supplier Material materials with Níquel of 4 - 5.5 % |
Otro | 0 - 0.5 % Show Supplier Material materials with Otro of 0 - 0.5 % |
Silicona | 0 - 0.25 % Show Supplier Material materials with Silicona of 0 - 0.25 % |
Zinc | 0 - 0.3 % Show Supplier Material materials with Zinc of 0 - 0.3 % |