General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Densidad of 2.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 70 [-] Show Supplier Material materials with Dureza Brinell of 70 [-] |
Elongación A5 | 23.0 °C | 17 % Show Supplier Material materials with Elongación A5 of 17 % |
Límite elástico Rp 0,2 | 23.0 °C | 125 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 125 MPa |
Módulo elástico | 23.0 °C | 71 GPa Show Supplier Material materials with Módulo elástico of 71 GPa |
Resistencia a la tracción | 23.0 °C | 275 MPa Show Supplier Material materials with Resistencia a la tracción of 275 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.38E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.38E-5 1/K |
Conductividad térmica | 23.0 °C | 110 W/(m·K) Show Supplier Material materials with Conductividad térmica of 110 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.60E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.60E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 92.4 - 95.6 % Show Supplier Material materials with Aluminio of 92.4 - 95.6 % |
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % |
Cromo | 0.05 - 0.25 % Show Supplier Material materials with Cromo of 0.05 - 0.25 % |
Hierro | 0.4 % Show Supplier Material materials with Hierro of 0.4 % |
Magnesio | 4 - 4.9 % Show Supplier Material materials with Magnesio of 4 - 4.9 % |
Manganeso | 0.4 - 1 % Show Supplier Material materials with Manganeso of 0.4 - 1 % |
Otro | 0.15 % Show Supplier Material materials with Otro of 0.15 % |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % |
Titanio | 0.15 % Show Supplier Material materials with Titanio of 0.15 % |
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % |