General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Densidad of 2.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 95 [-] Show Supplier Material materials with Dureza Brinell of 95 [-] |
Elongación A5 | 23.0 °C | 12 % Show Supplier Material materials with Elongación A5 of 12 % |
Límite elástico Rp 0,2 | 23.0 °C | 245 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 245 MPa |
Módulo elástico | 23.0 °C | 72 GPa Show Supplier Material materials with Módulo elástico of 72 GPa |
Resistencia a la tracción | 23.0 °C | 385 MPa Show Supplier Material materials with Resistencia a la tracción of 385 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.36E-5 1/K |
Conductividad térmica | 23.0 °C | 130 W/(m·K) Show Supplier Material materials with Conductividad térmica of 130 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.00E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.00E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Circonio | 0.25 % Show Supplier Material materials with Circonio of 0.25 % | max., Ti+Zr | |
Cobre | 3.5 - 4.5 % Show Supplier Material materials with Cobre of 3.5 - 4.5 % | ||
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % | ||
Hierro | 0.7 % Show Supplier Material materials with Hierro of 0.7 % | ||
Magnesio | 0.4 - 1 % Show Supplier Material materials with Magnesio of 0.4 - 1 % | ||
Manganeso | 0.4 - 1 % Show Supplier Material materials with Manganeso of 0.4 - 1 % | ||
Otro | 0.15 % Show Supplier Material materials with Otro of 0.15 % | total, each 0.05 | |
Silicona | 0.2 - 0.8 % Show Supplier Material materials with Silicona of 0.2 - 0.8 % | ||
Titanio | 0.25 % Show Supplier Material materials with Titanio of 0.25 % | max., Ti+Zr | |
Zinc | 0.25 % Show Supplier Material materials with Zinc of 0.25 % |