General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.7 g/cm³ Show Supplier Material materials with Densidad of 2.7 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 70 [-] Show Supplier Material materials with Dureza Brinell of 70 [-] |
Elongación A5 | 23.0 °C | 12 % Show Supplier Material materials with Elongación A5 of 12 % |
Límite elástico Rp 0,2 | 23.0 °C | 160 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 160 MPa |
Módulo elástico | 23.0 °C | 69 GPa Show Supplier Material materials with Módulo elástico of 69 GPa |
Resistencia a la tracción | 23.0 °C | 215 MPa Show Supplier Material materials with Resistencia a la tracción of 215 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.34E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.34E-5 1/K |
Conductividad térmica | 23.0 °C | 200 W/(m·K) Show Supplier Material materials with Conductividad térmica of 200 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 3.00E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 3.00E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % | ||
Cromo | 0.05 % Show Supplier Material materials with Cromo of 0.05 % | ||
Hierro | 0.1 - 0.3 % Show Supplier Material materials with Hierro of 0.1 - 0.3 % | ||
Magnesio | 0.35 - 0.6 % Show Supplier Material materials with Magnesio of 0.35 - 0.6 % | ||
Manganeso | 0.1 % Show Supplier Material materials with Manganeso of 0.1 % | ||
Otro | 0.15 % Show Supplier Material materials with Otro of 0.15 % | total, each 0.05 | |
Silicona | 0.3 - 0.6 % Show Supplier Material materials with Silicona of 0.3 - 0.6 % | ||
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % | ||
Zinc | 0.15 % Show Supplier Material materials with Zinc of 0.15 % |