General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Densidad of 2.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 115 [-] Show Supplier Material materials with Dureza Brinell of 115 [-] |
Elongación A5 | 23.0 °C | 10 % Show Supplier Material materials with Elongación A5 of 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 310 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 310 MPa |
Módulo elástico | 23.0 °C | 73 GPa Show Supplier Material materials with Módulo elástico of 73 GPa |
Resistencia a la tracción | 23.0 °C | 440 MPa Show Supplier Material materials with Resistencia a la tracción of 440 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.32E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.32E-5 1/K |
Conductividad térmica | 23.0 °C | 120 W/(m·K) Show Supplier Material materials with Conductividad térmica of 120 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 1.70E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 1.70E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 90.7 - 94.7 % Show Supplier Material materials with Aluminio of 90.7 - 94.7 % |
Circonio | 0 - 0.2 % Show Supplier Material materials with Circonio of 0 - 0.2 % |
Cobre | 3.8 - 4.9 % Show Supplier Material materials with Cobre of 3.8 - 4.9 % |
Cromo | 0 - 0.1 % Show Supplier Material materials with Cromo of 0 - 0.1 % |
Hierro | 0 - 0.5 % Show Supplier Material materials with Hierro of 0 - 0.5 % |
Magnesio | 1.2 - 1.8 % Show Supplier Material materials with Magnesio of 1.2 - 1.8 % |
Manganeso | 0.3 - 0.9 % Show Supplier Material materials with Manganeso of 0.3 - 0.9 % |
Otro | 0 - 0.15 % Show Supplier Material materials with Otro of 0 - 0.15 % |
Silicona | 0 - 0.5 % Show Supplier Material materials with Silicona of 0 - 0.5 % |
Titanio | 0 - 0.15 % Show Supplier Material materials with Titanio of 0 - 0.15 % |
Zinc | 0 - 0.25 % Show Supplier Material materials with Zinc of 0 - 0.25 % |