General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Densidad of 2.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 105 [-] Show Supplier Material materials with Dureza Brinell of 105 [-] |
Elongación A5 | 23.0 °C | 10 % Show Supplier Material materials with Elongación A5 of 10 % |
Límite elástico Rp 0,2 | 23.0 °C | 290 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 290 MPa |
Módulo elástico | 23.0 °C | 71 GPa Show Supplier Material materials with Módulo elástico of 71 GPa |
Resistencia a la tracción | 23.0 °C | 350 MPa Show Supplier Material materials with Resistencia a la tracción of 350 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.36E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.36E-5 1/K |
Conductividad térmica | 23.0 °C | 140 W/(m·K) Show Supplier Material materials with Conductividad térmica of 140 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.20E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.20E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Circonio | 0.08 - 0.2 % Show Supplier Material materials with Circonio of 0.08 - 0.2 % |
Cobre | 0.2 % Show Supplier Material materials with Cobre of 0.2 % |
Cromo | 0.35 % Show Supplier Material materials with Cromo of 0.35 % |
Hierro | 0.4 % Show Supplier Material materials with Hierro of 0.4 % |
Magnesio | 1.2 - 1.4 % Show Supplier Material materials with Magnesio of 1.2 - 1.4 % |
Manganeso | 0.05 - 0.5 % Show Supplier Material materials with Manganeso of 0.05 - 0.5 % |
Silicona | 0.35 % Show Supplier Material materials with Silicona of 0.35 % |
Titanio | 0.2 % Show Supplier Material materials with Titanio of 0.2 % |
Zinc | 4.5 - 5 % Show Supplier Material materials with Zinc of 4.5 - 5 % |