General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.9 g/cm³ Show Supplier Material materials with Densidad of 2.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 100 [-] Show Supplier Material materials with Dureza Brinell of 100 [-] |
Elongación A5 | 23.0 °C | 7 % Show Supplier Material materials with Elongación A5 of 7 % |
Límite elástico Rp 0,2 | 23.0 °C | 250 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 250 MPa |
Módulo elástico | 23.0 °C | 72 GPa Show Supplier Material materials with Módulo elástico of 72 GPa |
Resistencia a la tracción | 23.0 °C | 370 MPa Show Supplier Material materials with Resistencia a la tracción of 370 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.3E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.3E-5 1/K |
Conductividad térmica | 23.0 °C | 130 W/(m·K) Show Supplier Material materials with Conductividad térmica of 130 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.00E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.00E+7 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | Balance |
Bismuto | 0.2 % Show Supplier Material materials with Bismuto of 0.2 % |
Cobre | 3.3 - 4.6 % Show Supplier Material materials with Cobre of 3.3 - 4.6 % |
Cromo | 0.1 % Show Supplier Material materials with Cromo of 0.1 % |
Estaño | 0.2 % Show Supplier Material materials with Estaño of 0.2 % |
Hierro | 0.8 % Show Supplier Material materials with Hierro of 0.8 % |
Magnesio | 0.4 - 1.8 % Show Supplier Material materials with Magnesio of 0.4 - 1.8 % |
Manganeso | 0.5 - 1 % Show Supplier Material materials with Manganeso of 0.5 - 1 % |
Níquel | 0.2 % Show Supplier Material materials with Níquel of 0.2 % |
Plomo | 0.8 - 1.5 % Show Supplier Material materials with Plomo of 0.8 - 1.5 % |
Silicona | 0.8 % Show Supplier Material materials with Silicona of 0.8 % |
Titanio | 0.2 % Show Supplier Material materials with Titanio of 0.2 % |
Zinc | 0.8 % Show Supplier Material materials with Zinc of 0.8 % |