General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.8 g/cm³ Show Supplier Material materials with Densidad of 2.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 80 [-] Show Supplier Material materials with Dureza Brinell of 80 [-] |
Elongación A5 | 23.0 °C | 8 % Show Supplier Material materials with Elongación A5 of 8 % |
Límite elástico Rp 0,2 | 23.0 °C | 200 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 200 MPa |
Módulo elástico | 23.0 °C | 69 GPa Show Supplier Material materials with Módulo elástico of 69 GPa |
Resistencia a la tracción | 23.0 °C | 275 MPa Show Supplier Material materials with Resistencia a la tracción of 275 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 2.34E-5 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 2.34E-5 1/K |
Conductividad térmica | 23.0 °C | 170 W/(m·K) Show Supplier Material materials with Conductividad térmica of 170 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 23.0 °C | 2.60E+7 S/m Show Supplier Material materials with Conductividad eléctrica of 2.60E+7 S/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | Balance | ||
Bismuto | 0.7 % Show Supplier Material materials with Bismuto of 0.7 % | ||
Cobre | 0.1 % Show Supplier Material materials with Cobre of 0.1 % | ||
Cromo | 0.3 % Show Supplier Material materials with Cromo of 0.3 % | ||
Hierro | 0.5 % Show Supplier Material materials with Hierro of 0.5 % | ||
Magnesio | 0.6 - 1.2 % Show Supplier Material materials with Magnesio of 0.6 - 1.2 % | ||
Manganeso | 0.4 - 1 % Show Supplier Material materials with Manganeso of 0.4 - 1 % | ||
Otro | 0.15 % Show Supplier Material materials with Otro of 0.15 % | total, each 0.05 | |
Plomo | 0.4 - 2 % Show Supplier Material materials with Plomo of 0.4 - 2 % | ||
Silicona | 0.6 - 1.4 % Show Supplier Material materials with Silicona of 0.6 - 1.4 % | ||
Titanio | 0.2 % Show Supplier Material materials with Titanio of 0.2 % | ||
Zinc | 0.3 % Show Supplier Material materials with Zinc of 0.3 % |