General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 570 [-] Show Supplier Material materials with Dureza Brinell of 570 [-] | |
Elongación A5 | 23.0 °C | 10 % Show Supplier Material materials with Elongación A5 of 10 % | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 1300 - 1500 MPa Show Supplier Material materials with Resistencia a la tracción of 1300 - 1500 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbono | 0.15 % Show Supplier Material materials with Carbono of 0.15 % | max. |
Cromo | 16 - 19 % Show Supplier Material materials with Cromo of 16 - 19 % | |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % | max. |
Molibdeno | 0.8 % Show Supplier Material materials with Molibdeno of 0.8 % | |
Níquel | 6 - 9.5 % Show Supplier Material materials with Níquel of 6 - 9.5 % | |
Silicona | 2 % Show Supplier Material materials with Silicona of 2 % | max. |