General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Dureza Brinell of 215 [-] | |
Elongación A5 | 23.0 °C | 35 - 45 % Show Supplier Material materials with Elongación A5 of 35 - 45 % | |
Límite elástico Rp 0,2 | 23.0 °C | 190 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 190 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 500 - 700 MPa Show Supplier Material materials with Resistencia a la tracción of 500 - 700 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | max. |
Cromo | 17.5 - 19.5 % Show Supplier Material materials with Cromo of 17.5 - 19.5 % | |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % | max. |
Níquel | 8 - 10.5 % Show Supplier Material materials with Níquel of 8 - 10.5 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |