General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Dureza Brinell of 215 [-] | |
Elongación A5 | 23.0 °C | 30 - 40 % Show Supplier Material materials with Elongación A5 of 30 - 40 % | |
Límite elástico Rp 0,2 | 23.0 °C | 200 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 200 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 500 - 700 MPa Show Supplier Material materials with Resistencia a la tracción of 500 - 700 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % |
Cromo | 16 - 18.5 % Show Supplier Material materials with Cromo of 16 - 18.5 % |
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % |
Hierro | 62 - 72 % Show Supplier Material materials with Hierro of 62 - 72 % |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Molibdeno | 2 - 3 % Show Supplier Material materials with Molibdeno of 2 - 3 % |
Nitrógeno | 0.1 % Show Supplier Material materials with Nitrógeno of 0.1 % |
Níquel | 10 - 14 % Show Supplier Material materials with Níquel of 10 - 14 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |