Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Boro | 1.5E-3 - 5E-3 % Show Supplier Material materials with Boro of 1.5E-3 - 5E-3 % |
Carbono | 0.04 % Show Supplier Material materials with Carbono of 0.04 % |
Cromo | 16 - 18.5 % Show Supplier Material materials with Cromo of 16 - 18.5 % |
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % |
Hierro | 61.2 - 71.9 % Show Supplier Material materials with Hierro of 61.2 - 71.9 % |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Molibdeno | 2 - 3 % Show Supplier Material materials with Molibdeno of 2 - 3 % |
Nitrógeno | 0.1 - 0.22 % Show Supplier Material materials with Nitrógeno of 0.1 - 0.22 % |
Níquel | 10 - 14 % Show Supplier Material materials with Níquel of 10 - 14 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |