Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 215 [-] Show Supplier Material materials with Dureza Brinell of 215 [-] | |
Elongación A5 | 23.0 °C | 30 - 40 % Show Supplier Material materials with Elongación A5 of 30 - 40 % | |
Límite elástico Rp 0,2 | 23.0 °C | 190 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 190 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 500 - 700 MPa Show Supplier Material materials with Resistencia a la tracción of 500 - 700 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.4 % Show Supplier Material materials with Azufre of 0.4 % | |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. |
Cromo | 17 - 19 % Show Supplier Material materials with Cromo of 17 - 19 % | |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % | max. |
Níquel | 9 - 12 % Show Supplier Material materials with Níquel of 9 - 12 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |