Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | ||
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | ||
Cromo | 24 - 26 % Show Supplier Material materials with Cromo of 24 - 26 % | ||
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % | ||
Hierro | Balance | ||
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % | ||
Molibdeno | 1.2 - 2 % Show Supplier Material materials with Molibdeno of 1.2 - 2 % | ||
Nitrógeno | 0.14 - 0.2 % Show Supplier Material materials with Nitrógeno of 0.14 - 0.2 % | ||
Níquel | 5.5 - 6.5 % Show Supplier Material materials with Níquel of 5.5 - 6.5 % | ||
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |