Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0 - 0.03 % Show Supplier Material materials with Azufre of 0 - 0.03 % | |
Carbono | 0.08 - 0.15 % Show Supplier Material materials with Carbono of 0.08 - 0.15 % | |
Cromo | 11.5 - 13.5 % Show Supplier Material materials with Cromo of 11.5 - 13.5 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | |
Hierro | 83.1 - 88.4 % Show Supplier Material materials with Hierro of 83.1 - 88.4 % | |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Níquel | 0.75 % Show Supplier Material materials with Níquel of 0.75 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |