Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | ||
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | ||
Cromo | 11.5 - 13.5 % Show Supplier Material materials with Cromo of 11.5 - 13.5 % | ||
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | ||
Hierro | Balance | ||
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. | |
Níquel | 0.6 % Show Supplier Material materials with Níquel of 0.6 % | ||
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |