Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.15 - 0.35 % Show Supplier Material materials with Azufre of 0.15 - 0.35 % | |
Carbono | 0.15 % Show Supplier Material materials with Carbono of 0.15 % | |
Cromo | 12 - 14 % Show Supplier Material materials with Cromo of 12 - 14 % | |
Fósforo | 0.06 % Show Supplier Material materials with Fósforo of 0.06 % | |
Hierro | 82.4 - 87.9 % Show Supplier Material materials with Hierro of 82.4 - 87.9 % | |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Molibdeno | 0.6 % Show Supplier Material materials with Molibdeno of 0.6 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |