General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 220 [-] Show Supplier Material materials with Dureza Brinell of 220 [-] | |
Elongación A5 | 23.0 °C | 10 - 12 % Show Supplier Material materials with Elongación A5 of 10 - 12 % | |
Límite elástico Rp 0,2 | 23.0 °C | 500 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 500 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 650 - 850 MPa Show Supplier Material materials with Resistencia a la tracción of 650 - 850 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.15 - 0.35 % Show Supplier Material materials with Azufre of 0.15 - 0.35 % | |
Carbono | 0.17 % Show Supplier Material materials with Carbono of 0.17 % | |
Cromo | 15.5 - 17.5 % Show Supplier Material materials with Cromo of 15.5 - 17.5 % | |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Molibdeno | 0.2 - 0.6 % Show Supplier Material materials with Molibdeno of 0.2 - 0.6 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |