General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 295 [-] Show Supplier Material materials with Dureza Brinell of 295 [-] | |
Elongación A5 | 23.0 °C | 12 - 14 % Show Supplier Material materials with Elongación A5 of 12 - 14 % | |
Límite elástico Rp 0,2 | 23.0 °C | 600 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 600 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 800 - 950 MPa Show Supplier Material materials with Resistencia a la tracción of 800 - 950 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | |
Carbono | 0.22 % Show Supplier Material materials with Carbono of 0.22 % | |
Cromo | 15 - 17 % Show Supplier Material materials with Cromo of 15 - 17 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | |
Hierro | 77.7 - 83.8 % Show Supplier Material materials with Hierro of 77.7 - 83.8 % | |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Níquel | 1.3 - 2.5 % Show Supplier Material materials with Níquel of 1.3 - 2.5 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |