General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 265 [-] Show Supplier Material materials with Dureza Brinell of 265 [-] | |
Elongación A5 | 23.0 °C | 18 % Show Supplier Material materials with Elongación A5 of 18 % | |
Límite elástico Rp 0,2 | 23.0 °C | 430 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 430 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 730 - 750 MPa Show Supplier Material materials with Resistencia a la tracción of 730 - 750 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % | |
Carbono | 0.75 - 1 % Show Supplier Material materials with Carbono of 0.75 - 1 % | |
Cromo | 16 - 19 % Show Supplier Material materials with Cromo of 16 - 19 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | |
Hierro | 76.6 - 83.3 % Show Supplier Material materials with Hierro of 76.6 - 83.3 % | |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. |
Molibdeno | 1.3 % Show Supplier Material materials with Molibdeno of 1.3 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |
Vanadio | 0.07 - 0.12 % Show Supplier Material materials with Vanadio of 0.07 - 0.12 % |