General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 285 [-] Show Supplier Material materials with Dureza Brinell of 285 [-] | |
Elongación A5 | 23.0 °C | 13 % Show Supplier Material materials with Elongación A5 of 13 % | |
Límite elástico Rp 0,2 | 23.0 °C | 445 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 445 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 740 - 755 MPa Show Supplier Material materials with Resistencia a la tracción of 740 - 755 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % | |
Carbono | 1 - 1.2 % Show Supplier Material materials with Carbono of 1 - 1.2 % | |
Cromo | 16 - 18 % Show Supplier Material materials with Cromo of 16 - 18 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | |
Hierro | 78 - 83.1 % Show Supplier Material materials with Hierro of 78 - 83.1 % | |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. |
Molibdeno | 0.8 % Show Supplier Material materials with Molibdeno of 0.8 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |