General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 352 [-] Show Supplier Material materials with Dureza Brinell of 352 [-] | |
Elongación A5 | 23.0 °C | 12 % Show Supplier Material materials with Elongación A5 of 12 % | |
Límite elástico Rp 0,2 | 23.0 °C | 1000 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 1000 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 1070 - 1100 MPa Show Supplier Material materials with Resistencia a la tracción of 1070 - 1100 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | max. |
Cobre | 3 - 5 % Show Supplier Material materials with Cobre of 3 - 5 % | |
Cromo | 15 - 17 % Show Supplier Material materials with Cromo of 15 - 17 % | |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Molibdeno | 0 - 0.6 % Show Supplier Material materials with Molibdeno of 0 - 0.6 % | |
Niobio | 0 - 0.45 % Show Supplier Material materials with Niobio of 0 - 0.45 % | 5x%C |
Níquel | 3 - 5 % Show Supplier Material materials with Níquel of 3 - 5 % | |
Silicona | 0.7 % Show Supplier Material materials with Silicona of 0.7 % | max. |