Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.75 - 1.5 % Show Supplier Material materials with Aluminio of 0.75 - 1.5 % | |
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % | |
Carbono | 0.09 % Show Supplier Material materials with Carbono of 0.09 % | |
Cromo | 16 - 18 % Show Supplier Material materials with Cromo of 16 - 18 % | |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % | |
Hierro | 70.58 - 76.75 % Show Supplier Material materials with Hierro of 70.58 - 76.75 % | Balance |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | |
Níquel | 6.5 - 7.75 % Show Supplier Material materials with Níquel of 6.5 - 7.75 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |