Chemical properties
Property | Value |
---|---|
Aluminio | 0.75 - 1.5 % Show Supplier Material materials with Aluminio of 0.75 - 1.5 % |
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.09 % Show Supplier Material materials with Carbono of 0.09 % |
Cromo | 14 - 16 % Show Supplier Material materials with Cromo of 14 - 16 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Molibdeno | 2 - 3 % Show Supplier Material materials with Molibdeno of 2 - 3 % |
Níquel | 6.5 - 7.7 % Show Supplier Material materials with Níquel of 6.5 - 7.7 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |