Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Supplier Material materials with Azufre of 0.04 % |
Carbono | 0.02 % Show Supplier Material materials with Carbono of 0.02 % |
Cobre | 1 - 2 % Show Supplier Material materials with Cobre of 1 - 2 % |
Cromo | 19 - 23 % Show Supplier Material materials with Cromo of 19 - 23 % |
Fósforo | 0.05 % Show Supplier Material materials with Fósforo of 0.05 % |
Hierro | Balance |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % |
Molibdeno | 4 - 5 % Show Supplier Material materials with Molibdeno of 4 - 5 % |
Nitrógeno | 0.1 % Show Supplier Material materials with Nitrógeno of 0.1 % |
Níquel | 23 - 28 % Show Supplier Material materials with Níquel of 23 - 28 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |