General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 270 [-] Show Supplier Material materials with Dureza Brinell of 270 [-] | |
Elongación A5 | 23.0 °C | 25 % Show Supplier Material materials with Elongación A5 of 25 % | |
Límite elástico Rp 0,2 | 23.0 °C | 450 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 450 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 650 - 880 MPa Show Supplier Material materials with Resistencia a la tracción of 650 - 880 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Carbono | 0.03 % Show Supplier Material materials with Carbono of 0.03 % | max. |
Cromo | 21 - 23 % Show Supplier Material materials with Cromo of 21 - 23 % | |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % | max. |
Molibdeno | 2.5 - 3.5 % Show Supplier Material materials with Molibdeno of 2.5 - 3.5 % | |
Nitrógeno | 0.1 - 0.22 % Show Supplier Material materials with Nitrógeno of 0.1 - 0.22 % | |
Níquel | 4.5 - 6.5 % Show Supplier Material materials with Níquel of 4.5 - 6.5 % | |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % | max. |