Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 - 1 % Show Supplier Material materials with Aluminio of 0.5 - 1 % |
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % |
Carbono | 0.12 % Show Supplier Material materials with Carbono of 0.12 % |
Cromo | 6 - 8 % Show Supplier Material materials with Cromo of 6 - 8 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |