Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Supplier Material materials with Azufre of 0.03 % |
Carbono | 0.2 % Show Supplier Material materials with Carbono of 0.2 % |
Cromo | 23 - 27 % Show Supplier Material materials with Cromo of 23 - 27 % |
Fósforo | 0.04 % Show Supplier Material materials with Fósforo of 0.04 % |
Hierro | Balance |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % |
Nitrógeno | 0.25 % Show Supplier Material materials with Nitrógeno of 0.25 % |
Níquel | 0.75 % Show Supplier Material materials with Níquel of 0.75 % |
Silicona | 1 % Show Supplier Material materials with Silicona of 1 % |