General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Supplier Material materials with Densidad of 7.8 g/cm³ | typical for steels |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 192 [-] Show Supplier Material materials with Dureza Brinell of 192 [-] | |
Elongación A5 | 23.0 °C | 35 % Show Supplier Material materials with Elongación A5 of 35 % | |
Límite elástico Rp 0,2 | 23.0 °C | 210 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 210 MPa | |
Módulo elástico | 23.0 °C | 200 - 210 GPa Show Supplier Material materials with Módulo elástico of 200 - 210 GPa | typical for steels |
Resistencia a la tracción | 23.0 °C | 500 - 750 MPa Show Supplier Material materials with Resistencia a la tracción of 500 - 750 MPa |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0 - 0.75 % Show Supplier Material materials with Azufre of 0 - 0.75 % | |
Carbono | 0.15 % Show Supplier Material materials with Carbono of 0.15 % | max. |
Cromo | 24 - 26 % Show Supplier Material materials with Cromo of 24 - 26 % | |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % | max. |
Níquel | 19 - 22 % Show Supplier Material materials with Níquel of 19 - 22 % | |
Silicona | 1.5 % Show Supplier Material materials with Silicona of 1.5 % | max. |