Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.03 % Show Supplier Material materials with Azufre of 0 - 0.03 % |
Carbono | 0.05 - 0.12 % Show Supplier Material materials with Carbono of 0.05 - 0.12 % |
Cerio | 0.03 - 0.08 % Show Supplier Material materials with Cerio of 0.03 - 0.08 % |
Cromo | 20 - 22 % Show Supplier Material materials with Cromo of 20 - 22 % |
Fósforo | 0 - 0.05 % Show Supplier Material materials with Fósforo of 0 - 0.05 % |
Hierro | 62 - 68.4 % Show Supplier Material materials with Hierro of 62 - 68.4 % |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % |
Nitrógeno | 0.12 - 0.2 % Show Supplier Material materials with Nitrógeno of 0.12 - 0.2 % |
Níquel | 10 - 12 % Show Supplier Material materials with Níquel of 10 - 12 % |
Silicona | 1.4 - 2.5 % Show Supplier Material materials with Silicona of 1.4 - 2.5 % |