Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 23.0 °C | 190 [-] Show Supplier Material materials with Dureza Brinell of 190 [-] |
Elongación A5 | 23.0 °C | 20 - 24 % Show Supplier Material materials with Elongación A5 of 20 - 24 % |
Límite elástico Rp 0,2 | 23.0 °C | 275 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 275 MPa |
Resistencia a la tracción | 23.0 °C | 345 - 450 MPa Show Supplier Material materials with Resistencia a la tracción of 345 - 450 MPa |
Chemical properties
Property | Value |
---|---|
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % |
Hidrógeno | 0.02 % Show Supplier Material materials with Hidrógeno of 0.02 % |
Hierro | 0.3 % Show Supplier Material materials with Hierro of 0.3 % |
Nitrógeno | 0.03 % Show Supplier Material materials with Nitrógeno of 0.03 % |
Oxígeno | 0.25 % Show Supplier Material materials with Oxígeno of 0.25 % |
Titanio | Balance |