General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Densidad of 8.9 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 5E-3 % Show Supplier Material materials with Azufre of 5E-3 % | max. |
Carbono | 0.02 % Show Supplier Material materials with Carbono of 0.02 % | max. |
Cobre | 0.25 % Show Supplier Material materials with Cobre of 0.25 % | |
Hierro | 0.4 % Show Supplier Material materials with Hierro of 0.4 % | max. |
Magnesio | 0.15 % Show Supplier Material materials with Magnesio of 0.15 % | |
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % | max. |
Níquel | 99 % Show Supplier Material materials with Níquel of 99 % | min. |
Silicona | 0.25 % Show Supplier Material materials with Silicona of 0.25 % | max. |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % | max. |