General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 9.3 g/cm³ Show Supplier Material materials with Densidad of 9.3 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.1 - 0.5 % Show Supplier Material materials with Aluminio of 0.1 - 0.5 % | |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.01 % Show Supplier Material materials with Carbono of 0.01 % | max. |
Cobalto | 3 % Show Supplier Material materials with Cobalto of 3 % | max. |
Cobre | 0.5 % Show Supplier Material materials with Cobre of 0.5 % | |
Cromo | 0.5 - 3 % Show Supplier Material materials with Cromo of 0.5 - 3 % | |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. |
Hierro | 1 - 6 % Show Supplier Material materials with Hierro of 1 - 6 % | |
Manganeso | 3 % Show Supplier Material materials with Manganeso of 3 % | max. |
Molibdeno | 26 - 32 % Show Supplier Material materials with Molibdeno of 26 - 32 % | |
Níquel | 65 % Show Supplier Material materials with Níquel of 65 % | min. |
Otro | 0.4 % Show Supplier Material materials with Otro of 0.4 % | Nb + Ta |
Silicona | 0.1 % Show Supplier Material materials with Silicona of 0.1 % | max. |
Titanio | 0.2 % Show Supplier Material materials with Titanio of 0.2 % | max. |
Vanadio | 0.2 % Show Supplier Material materials with Vanadio of 0.2 % | |
Wolframio | 3 % Show Supplier Material materials with Wolframio of 3 % | max. |