General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Densidad of 8.9 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. | |
Carbono | 0.01 % Show Supplier Material materials with Carbono of 0.01 % | max. | |
Cobalto | 2.5 % Show Supplier Material materials with Cobalto of 2.5 % | max. | |
Cobre | 0.5 % Show Supplier Material materials with Cobre of 0.5 % | ||
Cromo | 14.5 - 16.5 % Show Supplier Material materials with Cromo of 14.5 - 16.5 % | ||
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. | |
Hierro | 4 - 7 % Show Supplier Material materials with Hierro of 4 - 7 % | ||
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. | |
Molibdeno | 15 - 17 % Show Supplier Material materials with Molibdeno of 15 - 17 % | ||
Níquel | balance | ||
Silicona | 0.08 % Show Supplier Material materials with Silicona of 0.08 % | max. | |
Vanadio | 0.35 % Show Supplier Material materials with Vanadio of 0.35 % | ||
Wolframio | 3 - 4.5 % Show Supplier Material materials with Wolframio of 3 - 4.5 % |