General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.6 g/cm³ Show Supplier Material materials with Densidad of 8.6 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.5 % Show Supplier Material materials with Aluminio of 0.5 % | max. | |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. | |
Carbono | 0.01 % Show Supplier Material materials with Carbono of 0.01 % | max. | |
Cobalto | 2 % Show Supplier Material materials with Cobalto of 2 % | max. | |
Cobre | 1.3 - 1.9 % Show Supplier Material materials with Cobre of 1.3 - 1.9 % | ||
Cromo | 22 - 24 % Show Supplier Material materials with Cromo of 22 - 24 % | ||
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. | |
Hierro | 3 % Show Supplier Material materials with Hierro of 3 % | max. | |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | max. | |
Molibdeno | 15 - 17 % Show Supplier Material materials with Molibdeno of 15 - 17 % | ||
Níquel | balance | ||
Silicona | 0.08 % Show Supplier Material materials with Silicona of 0.08 % | max. |