General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Supplier Material materials with Densidad of 8.9 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.5 % Show Supplier Material materials with Aluminio of 0.5 % | max. |
Azufre | 0.02 % Show Supplier Material materials with Azufre of 0.02 % | max. |
Carbono | 0.15 % Show Supplier Material materials with Carbono of 0.15 % | max. |
Cobre | 28 - 34 % Show Supplier Material materials with Cobre of 28 - 34 % | |
Hierro | 1 - 2.5 % Show Supplier Material materials with Hierro of 1 - 2.5 % | |
Manganeso | 2 % Show Supplier Material materials with Manganeso of 2 % | max. |
Níquel | 63 % Show Supplier Material materials with Níquel of 63 % | min. |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Titanio | 0.3 % Show Supplier Material materials with Titanio of 0.3 % | max. |