General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.5 g/cm³ Show Supplier Material materials with Densidad of 8.5 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 2.2 - 3.5 % Show Supplier Material materials with Aluminio of 2.2 - 3.5 % | |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.2 % Show Supplier Material materials with Carbono of 0.2 % | max. |
Cobre | 27 - 34 % Show Supplier Material materials with Cobre of 27 - 34 % | |
Hierro | 0.5 - 2 % Show Supplier Material materials with Hierro of 0.5 - 2 % | |
Manganeso | 1.5 % Show Supplier Material materials with Manganeso of 1.5 % | max. |
Níquel | 63 % Show Supplier Material materials with Níquel of 63 % | min. |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Titanio | 0.3 - 1 % Show Supplier Material materials with Titanio of 0.3 - 1 % |