General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.2 g/cm³ Show Supplier Material materials with Densidad of 8.2 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 1 - 1.7 % Show Supplier Material materials with Aluminio of 1 - 1.7 % | |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Boro | 6E-3 % Show Supplier Material materials with Boro of 6E-3 % | |
Carbono | 0.1 % Show Supplier Material materials with Carbono of 0.1 % | max. |
Cobre | 0.5 % Show Supplier Material materials with Cobre of 0.5 % | |
Cromo | 21 - 25 % Show Supplier Material materials with Cromo of 21 - 25 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Hierro | 18 % Show Supplier Material materials with Hierro of 18 % | max. |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. |
Níquel | 58 - 63 % Show Supplier Material materials with Níquel of 58 - 63 % | |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Titanio | 0.5 % Show Supplier Material materials with Titanio of 0.5 % | max. |