General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.5 g/cm³ Show Supplier Material materials with Densidad of 8.5 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.4 % Show Supplier Material materials with Aluminio of 0.4 % | max. |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.1 % Show Supplier Material materials with Carbono of 0.1 % | max. |
Cobalto | 1 % Show Supplier Material materials with Cobalto of 1 % | max. |
Cobre | 0.5 % Show Supplier Material materials with Cobre of 0.5 % | |
Cromo | 20 - 23 % Show Supplier Material materials with Cromo of 20 - 23 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Hierro | 5 % Show Supplier Material materials with Hierro of 5 % | max. |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | max. |
Molibdeno | 8 - 10 % Show Supplier Material materials with Molibdeno of 8 - 10 % | |
Níquel | 58 % Show Supplier Material materials with Níquel of 58 % | min. |
Otro | 3.15 - 4.15 % Show Supplier Material materials with Otro of 3.15 - 4.15 % | Nb + Ta |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Titanio | 0.4 % Show Supplier Material materials with Titanio of 0.4 % | max. |