General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Densidad of 8.3 g/cm³ |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.3 - 0.7 % Show Supplier Material materials with Aluminio of 0.3 - 0.7 % | ||
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. | |
Boro | 6E-3 % Show Supplier Material materials with Boro of 6E-3 % | ||
Carbono | 0.02 - 0.08 % Show Supplier Material materials with Carbono of 0.02 - 0.08 % | ||
Cobalto | 1 % Show Supplier Material materials with Cobalto of 1 % | max. | |
Cobre | 0.3 % Show Supplier Material materials with Cobre of 0.3 % | ||
Cromo | 17 - 21 % Show Supplier Material materials with Cromo of 17 - 21 % | ||
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. | |
Hierro | balance | ||
Manganeso | 0.35 % Show Supplier Material materials with Manganeso of 0.35 % | max. | |
Molibdeno | 2.8 - 3.3 % Show Supplier Material materials with Molibdeno of 2.8 - 3.3 % | ||
Níquel | 50 - 55 % Show Supplier Material materials with Níquel of 50 - 55 % | ||
Otro | 4.7 - 5.5 % Show Supplier Material materials with Otro of 4.7 - 5.5 % | Nb + Ta | |
Silicona | 0.35 % Show Supplier Material materials with Silicona of 0.35 % | max. | |
Titanio | 0.6 - 1.2 % Show Supplier Material materials with Titanio of 0.6 - 1.2 % |