General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.3 g/cm³ Show Supplier Material materials with Densidad of 8.3 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.4 - 1 % Show Supplier Material materials with Aluminio of 0.4 - 1 % | |
Azufre | 0.015 % Show Supplier Material materials with Azufre of 0.015 % | max. |
Carbono | 0.08 % Show Supplier Material materials with Carbono of 0.08 % | max. |
Cobalto | 1 % Show Supplier Material materials with Cobalto of 1 % | max. |
Cobre | 0.5 % Show Supplier Material materials with Cobre of 0.5 % | |
Cromo | 14 - 17 % Show Supplier Material materials with Cromo of 14 - 17 % | |
Fósforo | 0.02 % Show Supplier Material materials with Fósforo of 0.02 % | max. |
Hierro | 5 - 9 % Show Supplier Material materials with Hierro of 5 - 9 % | |
Manganeso | 1 % Show Supplier Material materials with Manganeso of 1 % | max. |
Níquel | 70 % Show Supplier Material materials with Níquel of 70 % | max. |
Otro | 0.7 - 1.2 % Show Supplier Material materials with Otro of 0.7 - 1.2 % | Nb + Ta |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Titanio | 2.25 - 2.75 % Show Supplier Material materials with Titanio of 2.25 - 2.75 % |